Hydrofluoric acid (HF) is a catalyst for the production of linear alkylbenzene (LAB). In this research, the corrosion and perforation in the overhead line of HF neutralization section in Bistoun Petrochemical Company (BPC), in Iran was investigated. The accumulation of sediment and under deposit corrosion has resulted in the perforation of the mentioned line. The main causes of failure were explored by visual checking, chemical characterizations, Scanning Electron Microscopy (SEM), and X-Ray Fluorescence (XRF). The effects of process conditions, pipeline design, water content, and oxygen amounts were studied. Corrosion and perforation in the line are based on the composition of the liquid or gases passing through the line and operating conditions. The reverse return of water vapors contaminated with KOH from the relief gas scrubber to the overhead line can accelerate the corrosion. Lastly, the suggestions have been proposed for troubleshooting, prevention from failure in the line, and HF leakage.
کلیدواژه ها:
نویسندگان
Aref Shokri
Department of Chemistry, Payame Noor University (PNU), Tehran, I.R. IRAN
مراجع و منابع این مقاله:
لیست زیر مراجع و منابع استفاده شده در این مقاله را نمایش می دهد. این مراجع به صورت کاملا ماشینی و بر اساس هوش مصنوعی استخراج شده اند و لذا ممکن است دارای اشکالاتی باشند که به مرور زمان دقت استخراج این محتوا افزایش می یابد. مراجعی که مقالات مربوط به آنها در سیویلیکا نمایه شده و پیدا شده اند، به خود مقاله لینک شده اند :