Delamination Wear Mechanism in Gray Cast Irons

سال انتشار: 1379
نوع سند: مقاله ژورنالی
زبان: انگلیسی
مشاهده: 153

فایل این مقاله در 14 صفحه با فرمت PDF قابل دریافت می باشد

استخراج به نرم افزارهای پژوهشی:

لینک ثابت به این مقاله:

شناسه ملی سند علمی:

JR_IJE-13-1_004

تاریخ نمایه سازی: 19 اسفند 1400

چکیده مقاله:

An investigation of the friction and sliding wear of gray cast iron against chromium plated cast irons was carried out on a newly constructed reciprocating friction and wear tester. The tests were the first to be done on the test rig under dry conditions and at the speed of ۱۷۰ cm/min, and variable loads of ۲۰-۲۶۰ N for a duration of ۱۵ min. to ۳ hours. The gray cast iron surfaces worn by a process of plastic deformation at the subsurface, crack nucleation, and crack growth leading to formation of plate like debris and therefore the delamination theory applies. No evidence of adhesion was observed. This could be due to formation of oxides on the wear surface which prevent adhesion. Channel type chromium plating 'picked' up cast iron from the counterbody surfaces by mechanically trapping cast iron debris on and within the cracks. The removal of the plated chromium left a pitted surface on the cast iron.

نویسندگان

M. Salehi

Mathematics, Isfahan University of Technology