The influence of Fe-rich intermetallics on the tensile properties and fracture behaviour of Al-Mg2Si metal matrix composite

سال انتشار: 1391
نوع سند: مقاله کنفرانسی
زبان: انگلیسی
مشاهده: 964

فایل این مقاله در 5 صفحه با فرمت PDF قابل دریافت می باشد

استخراج به نرم افزارهای پژوهشی:

لینک ثابت به این مقاله:

شناسه ملی سند علمی:

IIAC02_059

تاریخ نمایه سازی: 12 اردیبهشت 1392

چکیده مقاله:

In present research, an attempt was made to investigate the influence of different concentrations of Fe (0.5, 1, 1.5, 2 and 3 wt.%) on the tensile properties and fracture behaviour of in situ Al-15wt.%Mg2Si metal matrix composite. The composite ingots were made by casting process. In this work, the matrix composite were characterized by optical microscopy, scanning electron microscopy (SEM) and tensile tests experiment. The obtained results depicted optimum Fe (1 wt.%) levels for improving tensile properties. In the point of fracture behaviour, Fe-containing specimens showed a brittle mode of failure and acceptable cohesion between Mg2Si and matrix.

نویسندگان

R. Khorshidi

Faculty of Metallurgical and Materials Engineering, Semnan University, Semnan, P.O. Box: ۳۵۱۳۱-۱۹۱۱۱, Iran

M. Emamy

School of Metallurgy and Materials, University of Tehran, Tehran, P.O. Box: ۱۴۳۹۵-۷۳۱, Iran

S. Ghaiour

Faculty of Engineering, Islamic Azad University, Tehran, Iran

مراجع و منابع این مقاله:

لیست زیر مراجع و منابع استفاده شده در این مقاله را نمایش می دهد. این مراجع به صورت کاملا ماشینی و بر اساس هوش مصنوعی استخراج شده اند و لذا ممکن است دارای اشکالاتی باشند که به مرور زمان دقت استخراج این محتوا افزایش می یابد. مراجعی که مقالات مربوط به آنها در سیویلیکا نمایه شده و پیدا شده اند، به خود مقاله لینک شده اند :
  • of A1-P-T i-TiC-Nd, Oچ modifier on the microstructur [18] V. ...
  • R. Khorshidi, A. Honarbakhsh Raouf, M. Emamy, J. Campbell, "The ...
  • M. Emamy, R. Khorshidi, A. Honarbakhsh Raouf, "The influence of ...
  • Fig. 6. Fracture surface of Al- _ 5 %Mg, Si-2%Fe ...
  • A. Bahrami, A. Razaghian, M. Emamy, R. Khorshidi, «The effect ...
  • The effect of Fe content _ the tensile properties and ...
  • Y.G. Zhou, Q.D. Qin, W. Zhou, Y.H. Liang, ...
  • Tensile tests revealed optimum Fe level (1%) for _ Microstructue ...
  • Fe addition was a positive effect on the hardness [5] ...
  • _ The studies on the fracture surfaces revealed a brittle ...
  • Materials Science and Eng A. 447 (2007) 186-191. ...
  • %Fe content, a high density of Fe-rich intermetallic is observed. ...
  • C.L. Xu, H.Y. Wang, Y.F. Yang, Q.C. Jiang, :Effect Technol. ...
  • J. Zhang, Z. Fan, Y.Q. Wang, B.L. Zhou, [19] B. ...
  • Scripta Mater. 54 (2006) 1543-1548. ...
  • Q.D. Qin, Y.G. Zhao, C. Liu, P.J. Cong, W. Zhou, ...
  • Q.D. Qin, Y.G. Zhao, C. Liu, P.J. Cong, W. Zhou, ...
  • Q.D. Qin, Y.G. Zhao, P.J. Cong, Y.H. Liang, W. Chen, ...
  • Q.D. Qin, Y.G. Zhao, P.J. Cong, W. Zhou, B. Xu, ...
  • alloys by combined alloying of Fe and Cu", J Materials ...
  • K, TiF, ", J Materials Lett. 58 (2004) 2192-2194. ...
  • "Semisolid microstructue of Mg, Si/Al composite by [24] ASTM B557M-02a. ...
  • cooling slope cast and its evolution during partial testing wrought ...
  • C. Li, Y. Wu, H. Li, Y. Wu, X. Liu, ...
  • P. Ashtari, H. Tezuka, T. Sato, "Modification of Fe- [26] ...
  • containing intermetallic compounds by K addition to Fe- formation of ...
  • H.Y. Kim, T.Y. Park, S.W. Han, H.M. Lee, :Effects [27] ...
  • of Mn on the crystal structure of d-Al(Mn, Fe)Si particles ...
  • نمایش کامل مراجع