چکیده مقاله:
Microalloyed S۳۵۵N steel plates are extensively used in bridge and high-rise building structures. One of the factors affecting the mechanical properties is the size and morphology of inclusions. In this research, microalloyed S۳۵۵N steel plates with different sizes of inclusions were examined. One contained long manganese sulfide inclusions (LI material) and the other had short ones (SI material). Fatigue and tensile tests were carried out in through-thickness direction of both materials. Additionally, the fatigue test results were verified by “statistics of extreme value” (SEV) method. The tensile and fatigue tests revealed that toughness and fatigue limit of LI material were ۶۵% and ۳۰% less than those of SI, respectively. The SEV analysis conservatively predicted the fatigue limit of SI material. However, it was not accurate enough in the case of LI. These results could be explained using the behavior of manganese sulfide inclusions as short fatigue cracks in steels.
کلیدواژه ها:
fatigue ، Through-thickness direction ، Non-metallic inclusion ، Short fatigue crack ، Statistics of extreme value
نویسندگان
A. Abyazi
Faculty of Materials Engineering, Sahand University of Technology, Tabriz, ۵۳۳۱۷۱۱۱۱۱, Iran
A. Ebrahimi
Department of Mining and Metallurgical Engineering, Amirkabir University of Technology, Tehran, ۱۵۸۷۵۴۴۱۳, Iran