Effect of Damper Suction on Anode Spike and AnodeBurn off in Aluminium Electrochemical Cell (Case Study: South Hormoz Co)
- سال انتشار: 1397
- محل انتشار: پنجمین کنفرانس بین المللی آلومینیوم ایران
- کد COI اختصاصی: IIAC05_021
- زبان مقاله: انگلیسی
- تعداد مشاهده: 544
نویسندگان
Almahdi-South Hormoz Aluminium Smelter, Bandar abass, P.O. Box:۷۹۱۷۱-۷-۶۳۸۵, Iran
Almahdi-South Hormoz Aluminium Smelter, Bandar abass, P.O. Box:۷۹۱۷۱-۷-۶۳۸۵, Iran
چکیده
Nowadays, dry scrubber is very important in Hall–Héroult aluminum reduction technology, and despite the environmental impact and lower consumption of aluminum fluoride, the duct fan suction also affects on the pot performance and improves the surface temperature of the pot and increases production.During the production of 1 Kg aluminum, more than 1.2 kilograms of used material are converted to gas. Carbon dioxide and carbon monoxide are removed from the interior of the pot by means of the damper suction; and the anodes, which have high reactivity with carbon dioxide and air, lead to the pot blackness.Therefore, in the case of failure of the damper, the exiting of gas will be faced with problem and will lead to a series of events, which are discussed in this paper.At first, the output gas was measured using the pivot tube and then, the static pressure behind the damper was measured and its relationship with the number of spikes and burn off was studied apertures. Moreover, the quantity of dust output from main chimney of the dry purification system, and its effect on burn off and spike were studied.In this research, information were categorized and analyzed using Pivot tables in Excel software and data was compared with the data analysis tool in the Excel program and its correlation with other parameters and pot events was studied. The main reason of the spike is the free carbon inside the butt and the blackness. With the continuity of the blackness in the butt, this excess carbon is bound to the anode end, especially the end of cold anodes, and it intensifies the flow passing through the anode and accelerates the destruction process of the anode. The purpose of this study is to reduce production costsکلیدواژه ها
FTP,Anode burnoff, anode spike, aluminium smlterمقالات مرتبط جدید
- توسعه مبدل حرارتی داخلی ( IHX ) از طریق تغییر فرآیند ساخت و تولید لوله های گاز کولر در صنعت خودروسازی
- بهبودعملکرد سیکل تبرید تراکمی با تغییر فرآیند ساخت مبدل SLHX از آرایش مماسی به هم مرکز
- بررسی تاثیر لایه میانی روی در اتصال غیر مشابه آلیاژ پایه منیزیم AZ۳۱ و آلومینیوم ۶۰۶۱ به روش جوشکاری اصطکاکی اغتشاشی نقطهای
- بررسی تجربی سوراخکاری کامپوزیتهای پلیمری: مقایسه جوت و شیشه
- سیستم هوشمند پایش وضعیت بلبرینگ با استفاده از طیفنگاره صوتی جهت طبقهبندی و تشخیص خطای بلبرینگ ها
اطلاعات بیشتر در مورد COI
COI مخفف عبارت CIVILICA Object Identifier به معنی شناسه سیویلیکا برای اسناد است. COI کدی است که مطابق محل انتشار، به مقالات کنفرانسها و ژورنالهای داخل کشور به هنگام نمایه سازی بر روی پایگاه استنادی سیویلیکا اختصاص می یابد.
کد COI به مفهوم کد ملی اسناد نمایه شده در سیویلیکا است و کدی یکتا و ثابت است و به همین دلیل همواره قابلیت استناد و پیگیری دارد.