FTIR Study of SiO2 obtained from Rice Husk Ash

  • سال انتشار: 1393
  • محل انتشار: ششمین کنفرانس مهندسی برق و الکترونیک ایران
  • کد COI اختصاصی: ICEEE06_299
  • زبان مقاله: انگلیسی
  • تعداد مشاهده: 736
دانلود فایل این مقاله

نویسندگان

M.H Shahrokh Abadi

Electronic dept. of Electrical and Computer Engineering Faculty of Hakim Sabzevari University Sabzevar , Iran

Z Fakoor

Electronic dept. of Electrical and Computer Engineering Faculty of Hakim Sabzevari University Sabzevar , Iran

A Delbari

Electronic dept. of Electrical and Computer Engineering Faculty of Hakim Sabzevari University Sabzevar , Iran

چکیده

Silicon dioxide was produced from rice husk ash at elevated temperatures of 500°C for 4 hours and 45 minutes. The product was ground and then calcined at 600 and 800°C. The effects of the working temperature on the chemical bonding states of the powder of SiO2 were analyzed using FTIR spectroscopy. Infrared spectra from FTIR give valuable information on the structure of the products. It has been found that the both temperature and calcination time have a great directly impact on the formation of silicon dioxide.

کلیدواژه ها

Rice husk ash; Silicon Dioxide; FTIR; Crystalline

مقالات مرتبط جدید

اطلاعات بیشتر در مورد COI

COI مخفف عبارت CIVILICA Object Identifier به معنی شناسه سیویلیکا برای اسناد است. COI کدی است که مطابق محل انتشار، به مقالات کنفرانسها و ژورنالهای داخل کشور به هنگام نمایه سازی بر روی پایگاه استنادی سیویلیکا اختصاص می یابد.

کد COI به مفهوم کد ملی اسناد نمایه شده در سیویلیکا است و کدی یکتا و ثابت است و به همین دلیل همواره قابلیت استناد و پیگیری دارد.