The effect of supplementary process on grain size of boron carbide

  • سال انتشار: 1402
  • محل انتشار: اولین کنفرانس بین المللی علم و فناوری خوارزمی
  • کد COI اختصاصی: KHWARIZ01_087
  • زبان مقاله: انگلیسی
  • تعداد مشاهده: 98
دانلود فایل این مقاله

نویسندگان

Seyedeh Mina Saeedi Heydari

Assistant Prof., Department of Advanced Materials and Renewable Energies, Iranian Research Organization for Science andTechnology.

چکیده

In this paper, the effect of a supplementary process on the grain size of B۴C ceramic along with boronoxide and carbon impurities at various temperatures by pressureless sintering has been investigated. First, thesamples were subjected to uniaxial pressure and then were sintered by pressureless sintering method at ۲۱۰۰,۲۱۷۵, and ۲۲۵۰ °C. After that, the average grain size of the samples was calculated. The results of the samplesshowed that the supplementary washing process for removing boron oxide resulted in improved sinterabilityand reduced boron carbide grain size. Also, the presence of carbon in the primary powder increased sinterabilityand prevented the growth of the boron carbide grain.

کلیدواژه ها

Boron Carbide; Pressurless Sintering; Boron Oxide; Carbon; Average Grain Size

مقالات مرتبط جدید

اطلاعات بیشتر در مورد COI

COI مخفف عبارت CIVILICA Object Identifier به معنی شناسه سیویلیکا برای اسناد است. COI کدی است که مطابق محل انتشار، به مقالات کنفرانسها و ژورنالهای داخل کشور به هنگام نمایه سازی بر روی پایگاه استنادی سیویلیکا اختصاص می یابد.

کد COI به مفهوم کد ملی اسناد نمایه شده در سیویلیکا است و کدی یکتا و ثابت است و به همین دلیل همواره قابلیت استناد و پیگیری دارد.