Effect of Deposition Temperature on Nanostructure PbS Thin Films
- سال انتشار: 1391
- محل انتشار: اولین کنفرانس ملی نانوالکترونیک ایران
- کد COI اختصاصی: ICNE01_180
- زبان مقاله: انگلیسی
- تعداد مشاهده: 980
نویسندگان
Islamic Azad University, Urmia
چکیده
PbS/glass thin films with same deposition time of 80 min and two different deposition temperatures of room and 55oC, were produced by chemical bathdeposition method (CBD). Their nanostructures and surface morphology were investigated by using XRD (Xray diffraction) and AFM (Atomic force microscope). Theoptical properties were studied by spectrophotometer (in the wavelength range 380-800 nm) and consequentlywere discussed relation between deposition temperature and nanostructuresکلیدواژه ها
AFM, Deposition Temperature, Deposition Time, Lead Sulfide, Thin Films, XRDمقالات مرتبط جدید
- tGraph_PheroWalk : یک الگوریتم جدید برای یادگیری بازنمایی گراف های پویا
- Efficient Triple Modular Redundancy for Reliability Enhancement of DNNs Using Explainable AI
- مقایسه فناوری CMUT با پیزوالکتریک برای کاربرد در تصویربرداری التراسونیک
- بهبود کنترل دست رباتیک به کمک کنترل کننده تطبیقی فازی-PID
- طراحی و شبیه سازی آنتن تک قطبی چند بانده فشرده با تغذیه ریز نوار برای بهبود عملکرد در باندهای فرکانسی ۲.۵، ۳.۸، ۵.۴ و ۶.۹ گیگاهرتز
اطلاعات بیشتر در مورد COI
COI مخفف عبارت CIVILICA Object Identifier به معنی شناسه سیویلیکا برای اسناد است. COI کدی است که مطابق محل انتشار، به مقالات کنفرانسها و ژورنالهای داخل کشور به هنگام نمایه سازی بر روی پایگاه استنادی سیویلیکا اختصاص می یابد.
کد COI به مفهوم کد ملی اسناد نمایه شده در سیویلیکا است و کدی یکتا و ثابت است و به همین دلیل همواره قابلیت استناد و پیگیری دارد.